1. There are several experimental microscopy techniques for the calculation of dislocation density; but are there any reliable numerical ones, as well ? like those, which least include experimental parameters, except for some initial ones, like the initial density of dislocation, such as Reid's formula [1].
2. as a result of dislocation accumulation after deformation, slip bands form. are there any numerical techniques for slip band density estimation?
[1] Reid,N.C.,Gilbert,A., and Rosenfield,A.R.,1965, Phil. Mag.., 12, 409.