Poisson's ratio changable of carbon nanotube sheet

Submitted by Ying Li on

Here is a recent work on the Poisson's ratio of carbon nanotube sheet [1]. From the experimental results, the researchers found that the Poisson's ratio could change from 0.06 to -0.20 as the content of MWNTs increasing from 0~100%. The interesting zero Poisson's ratio and auxetic materials were thus found.  

Ref. [1] Sign Change of Poisson's Ratio for Carbon Nanotube Sheets. Science 25 April 2008: 504-507

Ying Li

Department of Engineering Mechanics, Tsinghua University

Buckling behavior of metal film/substrate structure under pure bending

Submitted by Ying Li on

Many studies on the thin film/substrate structure and its failure mechanism were reported in recent years. The direct experimental results of thin film/substrate structure by scanning electron microscopy (SEM) presents an intriguing problem:there exists a buckling failure mechanism at the lateral edge of metal film under pure bending. The qualitative theoretical analysis has been done on such buckling failure of thin film/substrate structure.

The free trial of Maney Publishing

Submitted by Ying Li on

Maney Publishing are pleased to announce that 30-day free trials are now available to individuals and institutions interested in our Materials Science and Engineering journals. To apply for a free trial simply follow the link and complete the online form. We will confirm your trial start date via e-mail and will be in contact with you prior to the expiration of your trial to answer any questions you may have.

著名力学家叶开沅先生逝世

Submitted by Ying Li on

我国著名力学家、中国力学学会原常务理事、甘肃省力学学会原理事长、甘肃省政协原常委

、甘肃省科协原常委、兰州大学力学专业和学科的创始人、兰州大学力学系首任主任、名誉

主任叶开沅先生因病医治无效,于2007年10月20日15时30分在北京不幸逝世,享年82岁。

  叶开沅,男,汉族,1926年5月19日出生于浙江省衢州市。1938年至1943年,在浙江省

立衢州中学学习。1944年,到北京灯市口育英中学学习。1945年考入北京大学土木工程系,

旋即转入燕京大学数学系学习。1946年,进入唐山工程学院学习,1947年转入清华大学电机

The US-China NSF Workshop and Summer Institute of Bio- and Nano-Mechanics and Applications (UCWSI2007)

Submitted by Ying Li on

The US-China NSF Workshop and Summer Institute of

Bio- and Nano-Mechanics and Applications (UCWSI2007)

August 31 -- September 4, 2007

Beijing, China

爆炸力学的发展史

Submitted by Ying Li on
爆炸力学是力学的一个分支,它主要研究爆炸的发生和发展规律,以及爆炸的力学效应的利用和防护的学科。它从力学角度研究化学爆炸、核爆炸、电爆炸、粒子束爆炸(也称辐射爆炸)、高速碰撞等能量突然释放或急剧转化的过程,以及由此产生的强冲击波(又称激波)、高速流动、大变形和破坏、抛掷等效应。自然界的雷电、地震、火山爆发、陨石碰撞、星体爆发等现象也可用爆炸力学方法来研究。