*Heading ** Job name: Tensile Model name: Model-1 ** Generated by: Abaqus/CAE 6.14-1 *Preprint, echo=NO, model=NO, history=NO, contact=NO ** ** PARTS ** *Part, name=Square *Node 1, 0., 0. 2, 5., 0. 3, 10., 0. 4, 0., 5. 5, 5., 5. 6, 10., 5. 7, 0., 10. 8, 5., 10. 9, 10., 10. *Element, type=CAX4RT 1, 1, 2, 5, 4 2, 2, 3, 6, 5 3, 4, 5, 8, 7 4, 5, 6, 9, 8 *Nset, nset=ALLND, generate 1, 9, 1 *Elset, elset=ALLEL, generate 1, 4, 1 ** Section: Section-1 *Solid Section, elset=ALLEL, material=Steel 1.0 *End Part ** ** ** ASSEMBLY ** *Assembly, name=Assembly ** *Instance, name=Square-1, part=Square *End Instance ** *Nset, nset=Set-left, instance=Square-1, generate 1, 7, 3 *Elset, elset=Set-left, instance=Square-1 1, 3 *Nset, nset=Set-bot, instance=Square-1, generate 1, 3, 1 *Elset, elset=Set-bot, instance=Square-1 1, 2 *Nset, nset=Set-right, instance=Square-1, generate 3, 9, 3 *Elset, elset=Set-right, instance=Square-1 2, 4 *Nset, nset=Set-top, instance=Square-1, generate 7, 9, 1 *Elset, elset=Set-top, instance=Square-1, generate 1, 4 *Nset, nset=Set-all, instance=Square-1, generate 1, 9, 1 *End Assembly *Amplitude, name=Amp-1 0., 0., 0.015, 1.5 ** ** MATERIALS ** *Material, name=Steel *Conductivity 34.0 *Density 7.83e-09 *Elastic 206000.0, 0.3 *Expansion 1.23e-05 *Inelastic Heat Fraction 0.9 *Plastic, hardening=JOHNSON COOK 806.0, 614.0, 0.168, 1.1, 1540., 20. *Rate Dependent, type=JOHNSON COOK 0.0089, 1.0 *Specific Heat 4.6e+08 ** ** PREDEFINED FIELDS ** ** Name: Predefined Field-1 Type: Temperature *Initial Conditions, type=TEMPERATURE Set-all, 20.0 ** ---------------------------------------------------------------- ** ** STEP: Step-1 ** *Step, name=Step-1, nlgeom=YES *Dynamic Temperature-displacement, Explicit, element by element , 0.01 *Bulk Viscosity 0.06, 1.2 ** ** BOUNDARY CONDITIONS ** ** Name: BC-1 Type: Displacement/Rotation *Boundary Set-left, 1, 1 Set-left, 2, 2 ** Name: BC-2 Type: Displacement/Rotation *Boundary Set-top, 2, 2 Set-bot, 2, 2 Set-right, 2, 2 ** Name: BC-4 Type: Displacement/Rotation *Boundary, amplitude=Amp-1 Set-right, 1, 1, 10.0 ** ** OUTPUT REQUESTS ** *Restart, write, number interval=1, time marks=NO ** ** FIELD OUTPUT: F-Output-1 ** *Output, field *Node Output A, RF, U, V *Element Output, directions=YES ER, ERV, EVF, LE, PE, PEEQ, PEEQVAVG, PEVAVG, S, SVAVG, TEMP, TEMPMAVG *Contact Output CSTRESS ** ** HISTORY OUTPUT: H-Output-1 ** *Output, history, variable=PRESELECT ** ** HISTORY OUTPUT: H-Output-2 ** *Output, history, time interval=1e-4 *Element Output, elset=Square-1.ALLEL MISES, S11, S22, S33, S12, PEEQ, TEMP, DENSITY *Incrementation Output DT *End Step