*Heading ** Job name: ENF#2-0 Model name: Model-1 ** Generated by: Abaqus/CAE 6.9-EF1 *Preprint, echo=NO, model=NO, history=NO, contact=NO ** ** PARTS ** *Part, name=Part-1 *Node 1, 0.0250000004, -0.0199999996, 0. 2, 0.0250000004, 0.00499999989, 0. 3, 0.0350000001, 0.00499999989, 0. 4, 0.0350000001, -0.0199999996, 0. 5, 0.0250000004, 0.00499999989, 0.00164999999 6, 0.0250000004, -0.0199999996, 0.00164999999 7, 0.0350000001, -0.0199999996, 0.00164999999 8, 0.0350000001, 0.00499999989, 0.00164999999 9, -0.275000006, 0.00499999989, 0.00164999999 10, -0.275000006, -0.0199999996, 0.00164999999 11, -0.125, -0.0199999996, 0.00164999999 12, -0.125, 0.00499999989, 0.00164999999 13, -0.275000006, -0.0199999996, -8.94069714e-12 14, -0.275000006, 0.00499999989, -8.94069714e-12 15, -0.125, 0.00499999989, -8.94069714e-12 16, -0.125, -0.0199999996, -8.94069714e-12 17, -0.284999996, -0.0199999996, 0. 18, -0.284999996, 0.00499999989, 0. 19, -0.284999996, 0.00499999989, 0.00164999999 20, -0.284999996, -0.0199999996, 0.00164999999 21, 0.0250000004, -0.0137499999, -4.47034857e-12 22, 0.0250000004, -0.00749999983, -4.47034857e-12 23, 0.0250000004, -0.00124999997, -4.47034857e-12 24, 0.0299999993, 0.00499999989, 0. 25, 0.0350000001, -0.00124999997, 0. 26, 0.0350000001, -0.00749999983, 0. 27, 0.0350000001, -0.0137499999, 0. 28, 0.0299999993, -0.0199999996, 0. 29, 0.0250000004, -0.00124999997, 0.00164999999 30, 0.0250000004, -0.00749999983, 0.00164999999 31, 0.0250000004, -0.0137499999, 0.00164999999 32, 0.0299999993, -0.0199999996, 0.00164999999 33, 0.0350000001, -0.0137499999, 0.00164999999 34, 0.0350000001, -0.00749999983, 0.00164999999 35, 0.0350000001, -0.00124999997, 0.00164999999 36, 0.0299999993, 0.00499999989, 0.00164999999 37, -0.275000006, -0.00124999997, 0.00164999999 38, -0.275000006, -0.00749999983, 0.00164999999 39, -0.275000006, -0.0137499999, 0.00164999999 40, -0.270000011, -0.0199999996, 0.00164999999 41, -0.264999986, -0.0199999996, 0.00164999999 42, -0.25999999, -0.0199999996, 0.00164999999 43, -0.254999995, -0.0199999996, 0.00164999999 44, -0.25, -0.0199999996, 0.00164999999 45, -0.245000005, -0.0199999996, 0.00164999999 46, -0.239999995, -0.0199999996, 0.00164999999 47, -0.234999999, -0.0199999996, 0.00164999999 48, -0.230000004, -0.0199999996, 0.00164999999 49, -0.224999994, -0.0199999996, 0.00164999999 50, -0.219999999, -0.0199999996, 0.00164999999 51, -0.215000004, -0.0199999996, 0.00164999999 52, -0.209999993, -0.0199999996, 0.00164999999 53, -0.204999998, -0.0199999996, 0.00164999999 54, -0.200000003, -0.0199999996, 0.00164999999 55, -0.194999993, -0.0199999996, 0.00164999999 56, -0.189999998, -0.0199999996, 0.00164999999 57, -0.185000002, -0.0199999996, 0.00164999999 58, -0.180000007, -0.0199999996, 0.00164999999 59, -0.174999997, -0.0199999996, 0.00164999999 60, -0.170000002, -0.0199999996, 0.00164999999 61, -0.165000007, -0.0199999996, 0.00164999999 62, -0.159999996, -0.0199999996, 0.00164999999 63, -0.155000001, -0.0199999996, 0.00164999999 64, -0.150000006, -0.0199999996, 0.00164999999 65, -0.144999996, -0.0199999996, 0.00164999999 66, -0.140000001, -0.0199999996, 0.00164999999 67, -0.135000005, -0.0199999996, 0.00164999999 68, -0.129999995, -0.0199999996, 0.00164999999 69, -0.125, -0.0137499999, 0.00164999999 70, -0.125, -0.00749999983, 0.00164999999 71, -0.125, -0.00124999997, 0.00164999999 72, -0.129999995, 0.00499999989, 0.00164999999 73, -0.135000005, 0.00499999989, 0.00164999999 74, -0.140000001, 0.00499999989, 0.00164999999 75, -0.144999996, 0.00499999989, 0.00164999999 76, -0.150000006, 0.00499999989, 0.00164999999 77, -0.155000001, 0.00499999989, 0.00164999999 78, -0.159999996, 0.00499999989, 0.00164999999 79, -0.165000007, 0.00499999989, 0.00164999999 80, -0.170000002, 0.00499999989, 0.00164999999 81, -0.174999997, 0.00499999989, 0.00164999999 82, -0.180000007, 0.00499999989, 0.00164999999 83, -0.185000002, 0.00499999989, 0.00164999999 84, -0.189999998, 0.00499999989, 0.00164999999 85, -0.194999993, 0.00499999989, 0.00164999999 86, -0.200000003, 0.00499999989, 0.00164999999 87, -0.204999998, 0.00499999989, 0.00164999999 88, -0.209999993, 0.00499999989, 0.00164999999 89, -0.215000004, 0.00499999989, 0.00164999999 90, -0.219999999, 0.00499999989, 0.00164999999 91, -0.224999994, 0.00499999989, 0.00164999999 92, -0.230000004, 0.00499999989, 0.00164999999 93, -0.234999999, 0.00499999989, 0.00164999999 94, -0.239999995, 0.00499999989, 0.00164999999 95, -0.245000005, 0.00499999989, 0.00164999999 96, -0.25, 0.00499999989, 0.00164999999 97, -0.254999995, 0.00499999989, 0.00164999999 98, -0.25999999, 0.00499999989, 0.00164999999 99, -0.264999986, 0.00499999989, 0.00164999999 100, -0.270000011, 0.00499999989, 0.00164999999 101, -0.275000006, -0.0137499999, -4.47034857e-12 102, -0.275000006, -0.00749999983, -4.47034857e-12 103, -0.275000006, -0.00124999997, -4.47034857e-12 104, -0.270000011, 0.00499999989, -8.94069714e-12 105, -0.264999986, 0.00499999989, -8.94069714e-12 106, -0.25999999, 0.00499999989, -8.94069714e-12 107, -0.254999995, 0.00499999989, -8.94069714e-12 108, -0.25, 0.00499999989, -8.94069714e-12 109, -0.245000005, 0.00499999989, -8.94069714e-12 110, -0.239999995, 0.00499999989, -8.94069714e-12 111, -0.234999999, 0.00499999989, -8.94069714e-12 112, -0.230000004, 0.00499999989, -8.94069714e-12 113, -0.224999994, 0.00499999989, -8.94069714e-12 114, -0.219999999, 0.00499999989, -8.94069714e-12 115, -0.215000004, 0.00499999989, -8.94069714e-12 116, -0.209999993, 0.00499999989, -8.94069714e-12 117, -0.204999998, 0.00499999989, -8.94069714e-12 118, -0.200000003, 0.00499999989, -8.94069714e-12 119, -0.194999993, 0.00499999989, -8.94069714e-12 120, -0.189999998, 0.00499999989, -8.94069714e-12 121, -0.185000002, 0.00499999989, -8.94069714e-12 122, -0.180000007, 0.00499999989, -8.94069714e-12 123, -0.174999997, 0.00499999989, -8.94069714e-12 124, -0.170000002, 0.00499999989, -8.94069714e-12 125, -0.165000007, 0.00499999989, -8.94069714e-12 126, -0.159999996, 0.00499999989, -8.94069714e-12 127, -0.155000001, 0.00499999989, -8.94069714e-12 128, -0.150000006, 0.00499999989, -8.94069714e-12 129, -0.144999996, 0.00499999989, -8.94069714e-12 130, -0.140000001, 0.00499999989, -8.94069714e-12 131, -0.135000005, 0.00499999989, -8.94069714e-12 132, -0.129999995, 0.00499999989, -8.94069714e-12 133, -0.125, -0.00124999997, -8.94069714e-12 134, -0.125, -0.00749999983, -8.94069714e-12 135, -0.125, -0.0137499999, -8.94069714e-12 136, -0.129999995, -0.0199999996, -8.94069714e-12 137, -0.135000005, -0.0199999996, -8.94069714e-12 138, -0.140000001, -0.0199999996, -8.94069714e-12 139, -0.144999996, -0.0199999996, -8.94069714e-12 140, -0.150000006, -0.0199999996, -8.94069714e-12 141, -0.155000001, -0.0199999996, -8.94069714e-12 142, -0.159999996, -0.0199999996, -8.94069714e-12 143, -0.165000007, -0.0199999996, -8.94069714e-12 144, -0.170000002, -0.0199999996, -8.94069714e-12 145, -0.174999997, -0.0199999996, -8.94069714e-12 146, -0.180000007, -0.0199999996, -8.94069714e-12 147, -0.185000002, -0.0199999996, -8.94069714e-12 148, -0.189999998, -0.0199999996, -8.94069714e-12 149, -0.194999993, -0.0199999996, -8.94069714e-12 150, -0.200000003, -0.0199999996, -8.94069714e-12 151, -0.204999998, -0.0199999996, -8.94069714e-12 152, -0.209999993, -0.0199999996, -8.94069714e-12 153, -0.215000004, -0.0199999996, -8.94069714e-12 154, -0.219999999, -0.0199999996, -8.94069714e-12 155, -0.224999994, -0.0199999996, -8.94069714e-12 156, -0.230000004, -0.0199999996, -8.94069714e-12 157, -0.234999999, -0.0199999996, -8.94069714e-12 158, -0.239999995, -0.0199999996, -8.94069714e-12 159, -0.245000005, -0.0199999996, -8.94069714e-12 160, -0.25, -0.0199999996, -8.94069714e-12 161, -0.254999995, -0.0199999996, -8.94069714e-12 162, -0.25999999, -0.0199999996, -8.94069714e-12 163, -0.264999986, -0.0199999996, -8.94069714e-12 164, -0.270000011, -0.0199999996, -8.94069714e-12 165, 0.0199999996, 0.00499999989, 0.00164999999 166, 0.0149999997, 0.00499999989, 0.00164999999 167, 0.00999999978, 0.00499999989, 0.00164999999 168, 0.00499999989, 0.00499999989, 0.00164999999 169, 0., 0.00499999989, 0.00164999999 170, -0.00499999989, 0.00499999989, 0.00164999999 171, -0.00999999978, 0.00499999989, 0.00164999999 172, -0.0149999997, 0.00499999989, 0.00164999999 173, -0.0199999996, 0.00499999989, 0.00164999999 174, -0.0250000004, 0.00499999989, 0.00164999999 175, -0.0299999993, 0.00499999989, 0.00164999999 176, -0.0350000001, 0.00499999989, 0.00164999999 177, -0.0399999991, 0.00499999989, 0.00164999999 178, -0.0450000018, 0.00499999989, 0.00164999999 179, -0.0500000007, 0.00499999989, 0.00164999999 180, -0.0549999997, 0.00499999989, 0.00164999999 181, -0.0599999987, 0.00499999989, 0.00164999999 182, -0.0649999976, 0.00499999989, 0.00164999999 183, -0.0700000003, 0.00499999989, 0.00164999999 184, -0.075000003, 0.00499999989, 0.00164999999 185, -0.0799999982, 0.00499999989, 0.00164999999 186, -0.0850000009, 0.00499999989, 0.00164999999 187, -0.0900000036, 0.00499999989, 0.00164999999 188, -0.0949999988, 0.00499999989, 0.00164999999 189, -0.100000001, 0.00499999989, 0.00164999999 190, -0.104999997, 0.00499999989, 0.00164999999 191, -0.109999999, 0.00499999989, 0.00164999999 192, -0.115000002, 0.00499999989, 0.00164999999 193, -0.119999997, 0.00499999989, 0.00164999999 194, -0.119999997, -0.0199999996, 0.00164999999 195, -0.115000002, -0.0199999996, 0.00164999999 196, -0.109999999, -0.0199999996, 0.00164999999 197, -0.104999997, -0.0199999996, 0.00164999999 198, -0.100000001, -0.0199999996, 0.00164999999 199, -0.0949999988, -0.0199999996, 0.00164999999 200, -0.0900000036, -0.0199999996, 0.00164999999 201, -0.0850000009, -0.0199999996, 0.00164999999 202, -0.0799999982, -0.0199999996, 0.00164999999 203, -0.075000003, -0.0199999996, 0.00164999999 204, -0.0700000003, -0.0199999996, 0.00164999999 205, -0.0649999976, -0.0199999996, 0.00164999999 206, -0.0599999987, -0.0199999996, 0.00164999999 207, -0.0549999997, -0.0199999996, 0.00164999999 208, -0.0500000007, -0.0199999996, 0.00164999999 209, -0.0450000018, -0.0199999996, 0.00164999999 210, -0.0399999991, -0.0199999996, 0.00164999999 211, -0.0350000001, -0.0199999996, 0.00164999999 212, -0.0299999993, -0.0199999996, 0.00164999999 213, -0.0250000004, -0.0199999996, 0.00164999999 214, -0.0199999996, -0.0199999996, 0.00164999999 215, -0.0149999997, -0.0199999996, 0.00164999999 216, -0.00999999978, -0.0199999996, 0.00164999999 217, -0.00499999989, -0.0199999996, 0.00164999999 218, 0., -0.0199999996, 0.00164999999 219, 0.00499999989, -0.0199999996, 0.00164999999 220, 0.00999999978, -0.0199999996, 0.00164999999 221, 0.0149999997, -0.0199999996, 0.00164999999 222, 0.0199999996, -0.0199999996, 0.00164999999 223, 0.0199999996, -0.0199999996, -8.94069714e-12 224, 0.0149999997, -0.0199999996, -8.94069714e-12 225, 0.00999999978, -0.0199999996, -8.94069714e-12 226, 0.00499999989, -0.0199999996, -8.94069714e-12 227, 0., -0.0199999996, -8.94069714e-12 228, -0.00499999989, -0.0199999996, -8.94069714e-12 229, -0.00999999978, -0.0199999996, -8.94069714e-12 230, -0.0149999997, -0.0199999996, -8.94069714e-12 231, -0.0199999996, -0.0199999996, -8.94069714e-12 232, -0.0250000004, -0.0199999996, -8.94069714e-12 233, -0.0299999993, -0.0199999996, -8.94069714e-12 234, -0.0350000001, -0.0199999996, -8.94069714e-12 235, -0.0399999991, -0.0199999996, -8.94069714e-12 236, -0.0450000018, -0.0199999996, -8.94069714e-12 237, -0.0500000007, -0.0199999996, -8.94069714e-12 238, -0.0549999997, -0.0199999996, -8.94069714e-12 239, -0.0599999987, -0.0199999996, -8.94069714e-12 240, -0.0649999976, -0.0199999996, -8.94069714e-12 241, -0.0700000003, -0.0199999996, -8.94069714e-12 242, -0.075000003, -0.0199999996, -8.94069714e-12 243, -0.0799999982, -0.0199999996, -8.94069714e-12 244, -0.0850000009, -0.0199999996, -8.94069714e-12 245, -0.0900000036, -0.0199999996, -8.94069714e-12 246, -0.0949999988, -0.0199999996, -8.94069714e-12 247, -0.100000001, -0.0199999996, -8.94069714e-12 248, -0.104999997, -0.0199999996, -8.94069714e-12 249, -0.109999999, -0.0199999996, -8.94069714e-12 250, -0.115000002, -0.0199999996, -8.94069714e-12 251, -0.119999997, -0.0199999996, -8.94069714e-12 252, -0.119999997, 0.00499999989, -8.94069714e-12 253, -0.115000002, 0.00499999989, -8.94069714e-12 254, -0.109999999, 0.00499999989, -8.94069714e-12 255, -0.104999997, 0.00499999989, -8.94069714e-12 256, -0.100000001, 0.00499999989, -8.94069714e-12 257, -0.0949999988, 0.00499999989, -8.94069714e-12 258, -0.0900000036, 0.00499999989, -8.94069714e-12 259, -0.0850000009, 0.00499999989, -8.94069714e-12 260, -0.0799999982, 0.00499999989, -8.94069714e-12 261, -0.075000003, 0.00499999989, -8.94069714e-12 262, -0.0700000003, 0.00499999989, -8.94069714e-12 263, -0.0649999976, 0.00499999989, -8.94069714e-12 264, -0.0599999987, 0.00499999989, -8.94069714e-12 265, -0.0549999997, 0.00499999989, -8.94069714e-12 266, -0.0500000007, 0.00499999989, -8.94069714e-12 267, -0.0450000018, 0.00499999989, -8.94069714e-12 268, -0.0399999991, 0.00499999989, -8.94069714e-12 269, -0.0350000001, 0.00499999989, -8.94069714e-12 270, -0.0299999993, 0.00499999989, -8.94069714e-12 271, -0.0250000004, 0.00499999989, -8.94069714e-12 272, -0.0199999996, 0.00499999989, -8.94069714e-12 273, -0.0149999997, 0.00499999989, -8.94069714e-12 274, -0.00999999978, 0.00499999989, -8.94069714e-12 275, -0.00499999989, 0.00499999989, -8.94069714e-12 276, 0., 0.00499999989, -8.94069714e-12 277, 0.00499999989, 0.00499999989, -8.94069714e-12 278, 0.00999999978, 0.00499999989, -8.94069714e-12 279, 0.0149999997, 0.00499999989, -8.94069714e-12 280, 0.0199999996, 0.00499999989, -8.94069714e-12 281, -0.280000001, -0.0199999996, 0. 282, -0.284999996, -0.0137499999, 0. 283, -0.284999996, -0.00749999983, 0. 284, -0.284999996, -0.00124999997, 0. 285, -0.280000001, 0.00499999989, 0. 286, -0.280000001, 0.00499999989, 0.00164999999 287, -0.284999996, -0.00124999997, 0.00164999999 288, -0.284999996, -0.00749999983, 0.00164999999 289, -0.284999996, -0.0137499999, 0.00164999999 290, -0.280000001, -0.0199999996, 0.00164999999 291, 0.0299999993, -0.0137499999, 0. 292, 0.0299999993, -0.00749999983, 0. 293, 0.0299999993, -0.00124999997, 0. 294, 0.0299999993, -0.0137499999, 0.00164999999 295, 0.0299999993, -0.00749999983, 0.00164999999 296, 0.0299999993, -0.00124999997, 0.00164999999 297, -0.270000011, -0.00124999997, 0.00164999999 298, -0.270000011, -0.00749999983, 0.00164999999 299, -0.270000011, -0.0137499999, 0.00164999999 300, -0.264999986, -0.00124999997, 0.00164999999 301, -0.264999986, -0.00749999983, 0.00164999999 302, -0.264999986, -0.0137499999, 0.00164999999 303, -0.25999999, -0.00124999997, 0.00164999999 304, -0.25999999, -0.00749999983, 0.00164999999 305, -0.25999999, -0.0137499999, 0.00164999999 306, -0.254999995, -0.00124999997, 0.00164999999 307, -0.254999995, -0.00749999983, 0.00164999999 308, -0.254999995, -0.0137499999, 0.00164999999 309, -0.25, -0.00124999997, 0.00164999999 310, -0.25, -0.00749999983, 0.00164999999 311, -0.25, -0.0137499999, 0.00164999999 312, -0.245000005, -0.00124999997, 0.00164999999 313, -0.245000005, -0.00749999983, 0.00164999999 314, -0.245000005, -0.0137499999, 0.00164999999 315, -0.239999995, -0.00124999997, 0.00164999999 316, -0.239999995, -0.00749999983, 0.00164999999 317, -0.239999995, -0.0137499999, 0.00164999999 318, -0.234999999, -0.00124999997, 0.00164999999 319, -0.234999999, -0.00749999983, 0.00164999999 320, -0.234999999, -0.0137499999, 0.00164999999 321, -0.230000004, -0.00124999997, 0.00164999999 322, -0.230000004, -0.00749999983, 0.00164999999 323, -0.230000004, -0.0137499999, 0.00164999999 324, -0.224999994, -0.00124999997, 0.00164999999 325, -0.224999994, -0.00749999983, 0.00164999999 326, -0.224999994, -0.0137499999, 0.00164999999 327, -0.219999999, -0.00124999997, 0.00164999999 328, -0.219999999, -0.00749999983, 0.00164999999 329, -0.219999999, -0.0137499999, 0.00164999999 330, -0.215000004, -0.00124999997, 0.00164999999 331, -0.215000004, -0.00749999983, 0.00164999999 332, -0.215000004, -0.0137499999, 0.00164999999 333, -0.209999993, -0.00124999997, 0.00164999999 334, -0.209999993, -0.00749999983, 0.00164999999 335, -0.209999993, -0.0137499999, 0.00164999999 336, -0.204999998, -0.00124999997, 0.00164999999 337, -0.204999998, -0.00749999983, 0.00164999999 338, -0.204999998, -0.0137499999, 0.00164999999 339, -0.200000003, -0.00124999997, 0.00164999999 340, -0.200000003, -0.00749999983, 0.00164999999 341, -0.200000003, -0.0137499999, 0.00164999999 342, -0.194999993, -0.00124999997, 0.00164999999 343, -0.194999993, -0.00749999983, 0.00164999999 344, -0.194999993, -0.0137499999, 0.00164999999 345, -0.189999998, -0.00124999997, 0.00164999999 346, -0.189999998, -0.00749999983, 0.00164999999 347, -0.189999998, -0.0137499999, 0.00164999999 348, -0.185000002, -0.00124999997, 0.00164999999 349, -0.185000002, -0.00749999983, 0.00164999999 350, -0.185000002, -0.0137499999, 0.00164999999 351, -0.180000007, -0.00124999997, 0.00164999999 352, -0.180000007, -0.00749999983, 0.00164999999 353, -0.180000007, -0.0137499999, 0.00164999999 354, -0.174999997, -0.00124999997, 0.00164999999 355, -0.174999997, -0.00749999983, 0.00164999999 356, -0.174999997, -0.0137499999, 0.00164999999 357, -0.170000002, -0.00124999997, 0.00164999999 358, -0.170000002, -0.00749999983, 0.00164999999 359, -0.170000002, -0.0137499999, 0.00164999999 360, -0.165000007, -0.00124999997, 0.00164999999 361, -0.165000007, -0.00749999983, 0.00164999999 362, -0.165000007, -0.0137499999, 0.00164999999 363, -0.159999996, -0.00124999997, 0.00164999999 364, -0.159999996, -0.00749999983, 0.00164999999 365, -0.159999996, -0.0137499999, 0.00164999999 366, -0.155000001, -0.00124999997, 0.00164999999 367, -0.155000001, -0.00749999983, 0.00164999999 368, -0.155000001, -0.0137499999, 0.00164999999 369, -0.150000006, -0.00124999997, 0.00164999999 370, -0.150000006, -0.00749999983, 0.00164999999 371, -0.150000006, -0.0137499999, 0.00164999999 372, -0.144999996, -0.00124999997, 0.00164999999 373, -0.144999996, -0.00749999983, 0.00164999999 374, -0.144999996, -0.0137499999, 0.00164999999 375, -0.140000001, -0.00124999997, 0.00164999999 376, -0.140000001, -0.00749999983, 0.00164999999 377, -0.140000001, -0.0137499999, 0.00164999999 378, -0.135000005, -0.00124999997, 0.00164999999 379, -0.135000005, -0.00749999983, 0.00164999999 380, -0.135000005, -0.0137499999, 0.00164999999 381, -0.129999995, -0.00124999997, 0.00164999999 382, -0.129999995, -0.00749999983, 0.00164999999 383, -0.129999995, -0.0137499999, 0.00164999999 384, -0.270000011, -0.00124999997, -8.94069714e-12 385, -0.270000011, -0.00749999983, -8.94069714e-12 386, -0.270000011, -0.0137499999, -8.94069714e-12 387, -0.264999986, -0.00124999997, -8.94069714e-12 388, -0.264999986, -0.00749999983, -8.94069714e-12 389, -0.264999986, -0.0137499999, -8.94069714e-12 390, -0.25999999, -0.00124999997, -8.94069714e-12 391, -0.25999999, -0.00749999983, -8.94069714e-12 392, -0.25999999, -0.0137499999, -8.94069714e-12 393, -0.254999995, -0.00124999997, -8.94069714e-12 394, -0.254999995, -0.00749999983, -8.94069714e-12 395, -0.254999995, -0.0137499999, -8.94069714e-12 396, -0.25, -0.00124999997, -8.94069714e-12 397, -0.25, -0.00749999983, -8.94069714e-12 398, -0.25, -0.0137499999, -8.94069714e-12 399, -0.245000005, -0.00124999997, -8.94069714e-12 400, -0.245000005, -0.00749999983, -8.94069714e-12 401, -0.245000005, -0.0137499999, -8.94069714e-12 402, -0.239999995, -0.00124999997, -8.94069714e-12 403, -0.239999995, -0.00749999983, -8.94069714e-12 404, -0.239999995, -0.0137499999, -8.94069714e-12 405, -0.234999999, -0.00124999997, -8.94069714e-12 406, -0.234999999, -0.00749999983, -8.94069714e-12 407, -0.234999999, -0.0137499999, -8.94069714e-12 408, -0.230000004, -0.00124999997, -8.94069714e-12 409, -0.230000004, -0.00749999983, -8.94069714e-12 410, -0.230000004, -0.0137499999, -8.94069714e-12 411, -0.224999994, -0.00124999997, -8.94069714e-12 412, -0.224999994, -0.00749999983, -8.94069714e-12 413, -0.224999994, -0.0137499999, -8.94069714e-12 414, -0.219999999, -0.00124999997, -8.94069714e-12 415, -0.219999999, -0.00749999983, -8.94069714e-12 416, -0.219999999, -0.0137499999, -8.94069714e-12 417, -0.215000004, -0.00124999997, -8.94069714e-12 418, -0.215000004, -0.00749999983, -8.94069714e-12 419, -0.215000004, -0.0137499999, -8.94069714e-12 420, -0.209999993, -0.00124999997, -8.94069714e-12 421, -0.209999993, -0.00749999983, -8.94069714e-12 422, -0.209999993, -0.0137499999, -8.94069714e-12 423, -0.204999998, -0.00124999997, -8.94069714e-12 424, -0.204999998, -0.00749999983, -8.94069714e-12 425, -0.204999998, -0.0137499999, -8.94069714e-12 426, -0.200000003, -0.00124999997, -8.94069714e-12 427, -0.200000003, -0.00749999983, -8.94069714e-12 428, -0.200000003, -0.0137499999, -8.94069714e-12 429, -0.194999993, -0.00124999997, -8.94069714e-12 430, -0.194999993, -0.00749999983, -8.94069714e-12 431, -0.194999993, -0.0137499999, -8.94069714e-12 432, -0.189999998, -0.00124999997, -8.94069714e-12 433, -0.189999998, -0.00749999983, -8.94069714e-12 434, -0.189999998, -0.0137499999, -8.94069714e-12 435, -0.185000002, -0.00124999997, -8.94069714e-12 436, -0.185000002, -0.00749999983, -8.94069714e-12 437, -0.185000002, -0.0137499999, -8.94069714e-12 438, -0.180000007, -0.00124999997, -8.94069714e-12 439, -0.180000007, -0.00749999983, -8.94069714e-12 440, -0.180000007, -0.0137499999, -8.94069714e-12 441, -0.174999997, -0.00124999997, -8.94069714e-12 442, -0.174999997, -0.00749999983, -8.94069714e-12 443, -0.174999997, -0.0137499999, -8.94069714e-12 444, -0.170000002, -0.00124999997, -8.94069714e-12 445, -0.170000002, -0.00749999983, -8.94069714e-12 446, -0.170000002, -0.0137499999, -8.94069714e-12 447, -0.165000007, -0.00124999997, -8.94069714e-12 448, -0.165000007, -0.00749999983, -8.94069714e-12 449, -0.165000007, -0.0137499999, -8.94069714e-12 450, -0.159999996, -0.00124999997, -8.94069714e-12 451, -0.159999996, -0.00749999983, -8.94069714e-12 452, -0.159999996, -0.0137499999, -8.94069714e-12 453, -0.155000001, -0.00124999997, -8.94069714e-12 454, -0.155000001, -0.00749999983, -8.94069714e-12 455, -0.155000001, -0.0137499999, -8.94069714e-12 456, -0.150000006, -0.00124999997, -8.94069714e-12 457, -0.150000006, -0.00749999983, -8.94069714e-12 458, -0.150000006, -0.0137499999, -8.94069714e-12 459, -0.144999996, -0.00124999997, -8.94069714e-12 460, -0.144999996, -0.00749999983, -8.94069714e-12 461, -0.144999996, -0.0137499999, -8.94069714e-12 462, -0.140000001, -0.00124999997, -8.94069714e-12 463, -0.140000001, -0.00749999983, -8.94069714e-12 464, -0.140000001, -0.0137499999, -8.94069714e-12 465, -0.135000005, -0.00124999997, -8.94069714e-12 466, -0.135000005, -0.00749999983, -8.94069714e-12 467, -0.135000005, -0.0137499999, -8.94069714e-12 468, -0.129999995, -0.00124999997, -8.94069714e-12 469, -0.129999995, -0.00749999983, -8.94069714e-12 470, -0.129999995, -0.0137499999, -8.94069714e-12 471, 0.0199999996, -0.0137499999, 0.00164999999 472, 0.0199999996, -0.00749999983, 0.00164999999 473, 0.0199999996, -0.00124999997, 0.00164999999 474, 0.0149999997, -0.0137499999, 0.00164999999 475, 0.0149999997, -0.00749999983, 0.00164999999 476, 0.0149999997, -0.00124999997, 0.00164999999 477, 0.00999999978, -0.0137499999, 0.00164999999 478, 0.00999999978, -0.00749999983, 0.00164999999 479, 0.00999999978, -0.00124999997, 0.00164999999 480, 0.00499999989, -0.0137499999, 0.00164999999 481, 0.00499999989, -0.00749999983, 0.00164999999 482, 0.00499999989, -0.00124999997, 0.00164999999 483, 0., -0.0137499999, 0.00164999999 484, 0., -0.00749999983, 0.00164999999 485, 0., -0.00124999997, 0.00164999999 486, -0.00499999989, -0.0137499999, 0.00164999999 487, -0.00499999989, -0.00749999983, 0.00164999999 488, -0.00499999989, -0.00124999997, 0.00164999999 489, -0.00999999978, -0.0137499999, 0.00164999999 490, -0.00999999978, -0.00749999983, 0.00164999999 491, -0.00999999978, -0.00124999997, 0.00164999999 492, -0.0149999997, -0.0137499999, 0.00164999999 493, -0.0149999997, -0.00749999983, 0.00164999999 494, -0.0149999997, -0.00124999997, 0.00164999999 495, -0.0199999996, -0.0137499999, 0.00164999999 496, -0.0199999996, -0.00749999983, 0.00164999999 497, -0.0199999996, -0.00124999997, 0.00164999999 498, -0.0250000004, -0.0137499999, 0.00164999999 499, -0.0250000004, -0.00749999983, 0.00164999999 500, -0.0250000004, -0.00124999997, 0.00164999999 501, -0.0299999993, -0.0137499999, 0.00164999999 502, -0.0299999993, -0.00749999983, 0.00164999999 503, -0.0299999993, -0.00124999997, 0.00164999999 504, -0.0350000001, -0.0137499999, 0.00164999999 505, -0.0350000001, -0.00749999983, 0.00164999999 506, -0.0350000001, -0.00124999997, 0.00164999999 507, -0.0399999991, -0.0137499999, 0.00164999999 508, -0.0399999991, -0.00749999983, 0.00164999999 509, -0.0399999991, -0.00124999997, 0.00164999999 510, -0.0450000018, -0.0137499999, 0.00164999999 511, -0.0450000018, -0.00749999983, 0.00164999999 512, -0.0450000018, -0.00124999997, 0.00164999999 513, -0.0500000007, -0.0137499999, 0.00164999999 514, -0.0500000007, -0.00749999983, 0.00164999999 515, -0.0500000007, -0.00124999997, 0.00164999999 516, -0.0549999997, -0.0137499999, 0.00164999999 517, -0.0549999997, -0.00749999983, 0.00164999999 518, -0.0549999997, -0.00124999997, 0.00164999999 519, -0.0599999987, -0.0137499999, 0.00164999999 520, -0.0599999987, -0.00749999983, 0.00164999999 521, -0.0599999987, -0.00124999997, 0.00164999999 522, -0.0649999976, -0.0137499999, 0.00164999999 523, -0.0649999976, -0.00749999983, 0.00164999999 524, -0.0649999976, -0.00124999997, 0.00164999999 525, -0.0700000003, -0.0137499999, 0.00164999999 526, -0.0700000003, -0.00749999983, 0.00164999999 527, -0.0700000003, -0.00124999997, 0.00164999999 528, -0.075000003, -0.0137499999, 0.00164999999 529, -0.075000003, -0.00749999983, 0.00164999999 530, -0.075000003, -0.00124999997, 0.00164999999 531, -0.0799999982, -0.0137499999, 0.00164999999 532, -0.0799999982, -0.00749999983, 0.00164999999 533, -0.0799999982, -0.00124999997, 0.00164999999 534, -0.0850000009, -0.0137499999, 0.00164999999 535, -0.0850000009, -0.00749999983, 0.00164999999 536, -0.0850000009, -0.00124999997, 0.00164999999 537, -0.0900000036, -0.0137499999, 0.00164999999 538, -0.0900000036, -0.00749999983, 0.00164999999 539, -0.0900000036, -0.00124999997, 0.00164999999 540, -0.0949999988, -0.0137499999, 0.00164999999 541, -0.0949999988, -0.00749999983, 0.00164999999 542, -0.0949999988, -0.00124999997, 0.00164999999 543, -0.100000001, -0.0137499999, 0.00164999999 544, -0.100000001, -0.00749999983, 0.00164999999 545, -0.100000001, -0.00124999997, 0.00164999999 546, -0.104999997, -0.0137499999, 0.00164999999 547, -0.104999997, -0.00749999983, 0.00164999999 548, -0.104999997, -0.00124999997, 0.00164999999 549, -0.109999999, -0.0137499999, 0.00164999999 550, -0.109999999, -0.00749999983, 0.00164999999 551, -0.109999999, -0.00124999997, 0.00164999999 552, -0.115000002, -0.0137499999, 0.00164999999 553, -0.115000002, -0.00749999983, 0.00164999999 554, -0.115000002, -0.00124999997, 0.00164999999 555, -0.119999997, -0.0137499999, 0.00164999999 556, -0.119999997, -0.00749999983, 0.00164999999 557, -0.119999997, -0.00124999997, 0.00164999999 558, 0.0199999996, -0.0137499999, -8.94069714e-12 559, 0.0199999996, -0.00749999983, -8.94069714e-12 560, 0.0199999996, -0.00124999997, -8.94069714e-12 561, 0.0149999997, -0.0137499999, -8.94069714e-12 562, 0.0149999997, -0.00749999983, -8.94069714e-12 563, 0.0149999997, -0.00124999997, -8.94069714e-12 564, 0.00999999978, -0.0137499999, -8.94069714e-12 565, 0.00999999978, -0.00749999983, -8.94069714e-12 566, 0.00999999978, -0.00124999997, -8.94069714e-12 567, 0.00499999989, -0.0137499999, -8.94069714e-12 568, 0.00499999989, -0.00749999983, -8.94069714e-12 569, 0.00499999989, -0.00124999997, -8.94069714e-12 570, 0., -0.0137499999, -8.94069714e-12 571, 0., -0.00749999983, -8.94069714e-12 572, 0., -0.00124999997, -8.94069714e-12 573, -0.00499999989, -0.0137499999, -8.94069714e-12 574, -0.00499999989, -0.00749999983, -8.94069714e-12 575, -0.00499999989, -0.00124999997, -8.94069714e-12 576, -0.00999999978, -0.0137499999, -8.94069714e-12 577, -0.00999999978, -0.00749999983, -8.94069714e-12 578, -0.00999999978, -0.00124999997, -8.94069714e-12 579, -0.0149999997, -0.0137499999, -8.94069714e-12 580, -0.0149999997, -0.00749999983, -8.94069714e-12 581, -0.0149999997, -0.00124999997, -8.94069714e-12 582, -0.0199999996, -0.0137499999, -8.94069714e-12 583, -0.0199999996, -0.00749999983, -8.94069714e-12 584, -0.0199999996, -0.00124999997, -8.94069714e-12 585, -0.0250000004, -0.0137499999, -8.94069714e-12 586, -0.0250000004, -0.00749999983, -8.94069714e-12 587, -0.0250000004, -0.00124999997, -8.94069714e-12 588, -0.0299999993, -0.0137499999, -8.94069714e-12 589, -0.0299999993, -0.00749999983, -8.94069714e-12 590, -0.0299999993, -0.00124999997, -8.94069714e-12 591, -0.0350000001, -0.0137499999, -8.94069714e-12 592, -0.0350000001, -0.00749999983, -8.94069714e-12 593, -0.0350000001, -0.00124999997, -8.94069714e-12 594, -0.0399999991, -0.0137499999, -8.94069714e-12 595, -0.0399999991, -0.00749999983, -8.94069714e-12 596, -0.0399999991, -0.00124999997, -8.94069714e-12 597, -0.0450000018, -0.0137499999, -8.94069714e-12 598, -0.0450000018, -0.00749999983, -8.94069714e-12 599, -0.0450000018, -0.00124999997, -8.94069714e-12 600, -0.0500000007, -0.0137499999, -8.94069714e-12 601, -0.0500000007, -0.00749999983, -8.94069714e-12 602, -0.0500000007, -0.00124999997, -8.94069714e-12 603, -0.0549999997, -0.0137499999, -8.94069714e-12 604, -0.0549999997, -0.00749999983, -8.94069714e-12 605, -0.0549999997, -0.00124999997, -8.94069714e-12 606, -0.0599999987, -0.0137499999, -8.94069714e-12 607, -0.0599999987, -0.00749999983, -8.94069714e-12 608, -0.0599999987, -0.00124999997, -8.94069714e-12 609, -0.0649999976, -0.0137499999, -8.94069714e-12 610, -0.0649999976, -0.00749999983, -8.94069714e-12 611, -0.0649999976, -0.00124999997, -8.94069714e-12 612, -0.0700000003, -0.0137499999, -8.94069714e-12 613, -0.0700000003, -0.00749999983, -8.94069714e-12 614, -0.0700000003, -0.00124999997, -8.94069714e-12 615, -0.075000003, -0.0137499999, -8.94069714e-12 616, -0.075000003, -0.00749999983, -8.94069714e-12 617, -0.075000003, -0.00124999997, -8.94069714e-12 618, -0.0799999982, -0.0137499999, -8.94069714e-12 619, -0.0799999982, -0.00749999983, -8.94069714e-12 620, -0.0799999982, -0.00124999997, -8.94069714e-12 621, -0.0850000009, -0.0137499999, -8.94069714e-12 622, -0.0850000009, -0.00749999983, -8.94069714e-12 623, -0.0850000009, -0.00124999997, -8.94069714e-12 624, -0.0900000036, -0.0137499999, -8.94069714e-12 625, -0.0900000036, -0.00749999983, -8.94069714e-12 626, -0.0900000036, -0.00124999997, -8.94069714e-12 627, -0.0949999988, -0.0137499999, -8.94069714e-12 628, -0.0949999988, -0.00749999983, -8.94069714e-12 629, -0.0949999988, -0.00124999997, -8.94069714e-12 630, -0.100000001, -0.0137499999, -8.94069714e-12 631, -0.100000001, -0.00749999983, -8.94069714e-12 632, -0.100000001, -0.00124999997, -8.94069714e-12 633, -0.104999997, -0.0137499999, -8.94069714e-12 634, -0.104999997, -0.00749999983, -8.94069714e-12 635, -0.104999997, -0.00124999997, -8.94069714e-12 636, -0.109999999, -0.0137499999, -8.94069714e-12 637, -0.109999999, -0.00749999983, -8.94069714e-12 638, -0.109999999, -0.00124999997, -8.94069714e-12 639, -0.115000002, -0.0137499999, -8.94069714e-12 640, -0.115000002, -0.00749999983, -8.94069714e-12 641, -0.115000002, -0.00124999997, -8.94069714e-12 642, -0.119999997, -0.0137499999, -8.94069714e-12 643, -0.119999997, -0.00749999983, -8.94069714e-12 644, -0.119999997, -0.00124999997, -8.94069714e-12 645, -0.280000001, -0.00124999997, 0. 646, -0.280000001, -0.00749999983, 0. 647, -0.280000001, -0.0137499999, 0. 648, -0.280000001, -0.00124999997, 0.00164999999 649, -0.280000001, -0.00749999983, 0.00164999999 650, -0.280000001, -0.0137499999, 0.00164999999 *Element, type=SC8R 1, 28, 291, 21, 1, 32, 294, 31, 6 2, 291, 292, 22, 21, 294, 295, 30, 31 3, 292, 293, 23, 22, 295, 296, 29, 30 4, 293, 24, 2, 23, 296, 36, 5, 29 5, 4, 27, 291, 28, 7, 33, 294, 32 6, 27, 26, 292, 291, 33, 34, 295, 294 7, 26, 25, 293, 292, 34, 35, 296, 295 8, 25, 3, 24, 293, 35, 8, 36, 296 9, 100, 297, 37, 9, 104, 384, 103, 14 10, 297, 298, 38, 37, 384, 385, 102, 103 11, 298, 299, 39, 38, 385, 386, 101, 102 12, 299, 40, 10, 39, 386, 164, 13, 101 13, 99, 300, 297, 100, 105, 387, 384, 104 14, 300, 301, 298, 297, 387, 388, 385, 384 15, 301, 302, 299, 298, 388, 389, 386, 385 16, 302, 41, 40, 299, 389, 163, 164, 386 17, 98, 303, 300, 99, 106, 390, 387, 105 18, 303, 304, 301, 300, 390, 391, 388, 387 19, 304, 305, 302, 301, 391, 392, 389, 388 20, 305, 42, 41, 302, 392, 162, 163, 389 21, 97, 306, 303, 98, 107, 393, 390, 106 22, 306, 307, 304, 303, 393, 394, 391, 390 23, 307, 308, 305, 304, 394, 395, 392, 391 24, 308, 43, 42, 305, 395, 161, 162, 392 25, 96, 309, 306, 97, 108, 396, 393, 107 26, 309, 310, 307, 306, 396, 397, 394, 393 27, 310, 311, 308, 307, 397, 398, 395, 394 28, 311, 44, 43, 308, 398, 160, 161, 395 29, 95, 312, 309, 96, 109, 399, 396, 108 30, 312, 313, 310, 309, 399, 400, 397, 396 31, 313, 314, 311, 310, 400, 401, 398, 397 32, 314, 45, 44, 311, 401, 159, 160, 398 33, 94, 315, 312, 95, 110, 402, 399, 109 34, 315, 316, 313, 312, 402, 403, 400, 399 35, 316, 317, 314, 313, 403, 404, 401, 400 36, 317, 46, 45, 314, 404, 158, 159, 401 37, 93, 318, 315, 94, 111, 405, 402, 110 38, 318, 319, 316, 315, 405, 406, 403, 402 39, 319, 320, 317, 316, 406, 407, 404, 403 40, 320, 47, 46, 317, 407, 157, 158, 404 41, 92, 321, 318, 93, 112, 408, 405, 111 42, 321, 322, 319, 318, 408, 409, 406, 405 43, 322, 323, 320, 319, 409, 410, 407, 406 44, 323, 48, 47, 320, 410, 156, 157, 407 45, 91, 324, 321, 92, 113, 411, 408, 112 46, 324, 325, 322, 321, 411, 412, 409, 408 47, 325, 326, 323, 322, 412, 413, 410, 409 48, 326, 49, 48, 323, 413, 155, 156, 410 49, 90, 327, 324, 91, 114, 414, 411, 113 50, 327, 328, 325, 324, 414, 415, 412, 411 51, 328, 329, 326, 325, 415, 416, 413, 412 52, 329, 50, 49, 326, 416, 154, 155, 413 53, 89, 330, 327, 90, 115, 417, 414, 114 54, 330, 331, 328, 327, 417, 418, 415, 414 55, 331, 332, 329, 328, 418, 419, 416, 415 56, 332, 51, 50, 329, 419, 153, 154, 416 57, 88, 333, 330, 89, 116, 420, 417, 115 58, 333, 334, 331, 330, 420, 421, 418, 417 59, 334, 335, 332, 331, 421, 422, 419, 418 60, 335, 52, 51, 332, 422, 152, 153, 419 61, 87, 336, 333, 88, 117, 423, 420, 116 62, 336, 337, 334, 333, 423, 424, 421, 420 63, 337, 338, 335, 334, 424, 425, 422, 421 64, 338, 53, 52, 335, 425, 151, 152, 422 65, 86, 339, 336, 87, 118, 426, 423, 117 66, 339, 340, 337, 336, 426, 427, 424, 423 67, 340, 341, 338, 337, 427, 428, 425, 424 68, 341, 54, 53, 338, 428, 150, 151, 425 69, 85, 342, 339, 86, 119, 429, 426, 118 70, 342, 343, 340, 339, 429, 430, 427, 426 71, 343, 344, 341, 340, 430, 431, 428, 427 72, 344, 55, 54, 341, 431, 149, 150, 428 73, 84, 345, 342, 85, 120, 432, 429, 119 74, 345, 346, 343, 342, 432, 433, 430, 429 75, 346, 347, 344, 343, 433, 434, 431, 430 76, 347, 56, 55, 344, 434, 148, 149, 431 77, 83, 348, 345, 84, 121, 435, 432, 120 78, 348, 349, 346, 345, 435, 436, 433, 432 79, 349, 350, 347, 346, 436, 437, 434, 433 80, 350, 57, 56, 347, 437, 147, 148, 434 81, 82, 351, 348, 83, 122, 438, 435, 121 82, 351, 352, 349, 348, 438, 439, 436, 435 83, 352, 353, 350, 349, 439, 440, 437, 436 84, 353, 58, 57, 350, 440, 146, 147, 437 85, 81, 354, 351, 82, 123, 441, 438, 122 86, 354, 355, 352, 351, 441, 442, 439, 438 87, 355, 356, 353, 352, 442, 443, 440, 439 88, 356, 59, 58, 353, 443, 145, 146, 440 89, 80, 357, 354, 81, 124, 444, 441, 123 90, 357, 358, 355, 354, 444, 445, 442, 441 91, 358, 359, 356, 355, 445, 446, 443, 442 92, 359, 60, 59, 356, 446, 144, 145, 443 93, 79, 360, 357, 80, 125, 447, 444, 124 94, 360, 361, 358, 357, 447, 448, 445, 444 95, 361, 362, 359, 358, 448, 449, 446, 445 96, 362, 61, 60, 359, 449, 143, 144, 446 97, 78, 363, 360, 79, 126, 450, 447, 125 98, 363, 364, 361, 360, 450, 451, 448, 447 99, 364, 365, 362, 361, 451, 452, 449, 448 100, 365, 62, 61, 362, 452, 142, 143, 449 101, 77, 366, 363, 78, 127, 453, 450, 126 102, 366, 367, 364, 363, 453, 454, 451, 450 103, 367, 368, 365, 364, 454, 455, 452, 451 104, 368, 63, 62, 365, 455, 141, 142, 452 105, 76, 369, 366, 77, 128, 456, 453, 127 106, 369, 370, 367, 366, 456, 457, 454, 453 107, 370, 371, 368, 367, 457, 458, 455, 454 108, 371, 64, 63, 368, 458, 140, 141, 455 109, 75, 372, 369, 76, 129, 459, 456, 128 110, 372, 373, 370, 369, 459, 460, 457, 456 111, 373, 374, 371, 370, 460, 461, 458, 457 112, 374, 65, 64, 371, 461, 139, 140, 458 113, 74, 375, 372, 75, 130, 462, 459, 129 114, 375, 376, 373, 372, 462, 463, 460, 459 115, 376, 377, 374, 373, 463, 464, 461, 460 116, 377, 66, 65, 374, 464, 138, 139, 461 117, 73, 378, 375, 74, 131, 465, 462, 130 118, 378, 379, 376, 375, 465, 466, 463, 462 119, 379, 380, 377, 376, 466, 467, 464, 463 120, 380, 67, 66, 377, 467, 137, 138, 464 121, 72, 381, 378, 73, 132, 468, 465, 131 122, 381, 382, 379, 378, 468, 469, 466, 465 123, 382, 383, 380, 379, 469, 470, 467, 466 124, 383, 68, 67, 380, 470, 136, 137, 467 125, 12, 71, 381, 72, 15, 133, 468, 132 126, 71, 70, 382, 381, 133, 134, 469, 468 127, 70, 69, 383, 382, 134, 135, 470, 469 128, 69, 11, 68, 383, 135, 16, 136, 470 129, 222, 471, 31, 6, 223, 558, 21, 1 130, 471, 472, 30, 31, 558, 559, 22, 21 131, 472, 473, 29, 30, 559, 560, 23, 22 132, 473, 165, 5, 29, 560, 280, 2, 23 133, 221, 474, 471, 222, 224, 561, 558, 223 134, 474, 475, 472, 471, 561, 562, 559, 558 135, 475, 476, 473, 472, 562, 563, 560, 559 136, 476, 166, 165, 473, 563, 279, 280, 560 137, 220, 477, 474, 221, 225, 564, 561, 224 138, 477, 478, 475, 474, 564, 565, 562, 561 139, 478, 479, 476, 475, 565, 566, 563, 562 140, 479, 167, 166, 476, 566, 278, 279, 563 141, 219, 480, 477, 220, 226, 567, 564, 225 142, 480, 481, 478, 477, 567, 568, 565, 564 143, 481, 482, 479, 478, 568, 569, 566, 565 144, 482, 168, 167, 479, 569, 277, 278, 566 145, 218, 483, 480, 219, 227, 570, 567, 226 146, 483, 484, 481, 480, 570, 571, 568, 567 147, 484, 485, 482, 481, 571, 572, 569, 568 148, 485, 169, 168, 482, 572, 276, 277, 569 149, 217, 486, 483, 218, 228, 573, 570, 227 150, 486, 487, 484, 483, 573, 574, 571, 570 151, 487, 488, 485, 484, 574, 575, 572, 571 152, 488, 170, 169, 485, 575, 275, 276, 572 153, 216, 489, 486, 217, 229, 576, 573, 228 154, 489, 490, 487, 486, 576, 577, 574, 573 155, 490, 491, 488, 487, 577, 578, 575, 574 156, 491, 171, 170, 488, 578, 274, 275, 575 157, 215, 492, 489, 216, 230, 579, 576, 229 158, 492, 493, 490, 489, 579, 580, 577, 576 159, 493, 494, 491, 490, 580, 581, 578, 577 160, 494, 172, 171, 491, 581, 273, 274, 578 161, 214, 495, 492, 215, 231, 582, 579, 230 162, 495, 496, 493, 492, 582, 583, 580, 579 163, 496, 497, 494, 493, 583, 584, 581, 580 164, 497, 173, 172, 494, 584, 272, 273, 581 165, 213, 498, 495, 214, 232, 585, 582, 231 166, 498, 499, 496, 495, 585, 586, 583, 582 167, 499, 500, 497, 496, 586, 587, 584, 583 168, 500, 174, 173, 497, 587, 271, 272, 584 169, 212, 501, 498, 213, 233, 588, 585, 232 170, 501, 502, 499, 498, 588, 589, 586, 585 171, 502, 503, 500, 499, 589, 590, 587, 586 172, 503, 175, 174, 500, 590, 270, 271, 587 173, 211, 504, 501, 212, 234, 591, 588, 233 174, 504, 505, 502, 501, 591, 592, 589, 588 175, 505, 506, 503, 502, 592, 593, 590, 589 176, 506, 176, 175, 503, 593, 269, 270, 590 177, 210, 507, 504, 211, 235, 594, 591, 234 178, 507, 508, 505, 504, 594, 595, 592, 591 179, 508, 509, 506, 505, 595, 596, 593, 592 180, 509, 177, 176, 506, 596, 268, 269, 593 181, 209, 510, 507, 210, 236, 597, 594, 235 182, 510, 511, 508, 507, 597, 598, 595, 594 183, 511, 512, 509, 508, 598, 599, 596, 595 184, 512, 178, 177, 509, 599, 267, 268, 596 185, 208, 513, 510, 209, 237, 600, 597, 236 186, 513, 514, 511, 510, 600, 601, 598, 597 187, 514, 515, 512, 511, 601, 602, 599, 598 188, 515, 179, 178, 512, 602, 266, 267, 599 189, 207, 516, 513, 208, 238, 603, 600, 237 190, 516, 517, 514, 513, 603, 604, 601, 600 191, 517, 518, 515, 514, 604, 605, 602, 601 192, 518, 180, 179, 515, 605, 265, 266, 602 193, 206, 519, 516, 207, 239, 606, 603, 238 194, 519, 520, 517, 516, 606, 607, 604, 603 195, 520, 521, 518, 517, 607, 608, 605, 604 196, 521, 181, 180, 518, 608, 264, 265, 605 197, 205, 522, 519, 206, 240, 609, 606, 239 198, 522, 523, 520, 519, 609, 610, 607, 606 199, 523, 524, 521, 520, 610, 611, 608, 607 200, 524, 182, 181, 521, 611, 263, 264, 608 201, 204, 525, 522, 205, 241, 612, 609, 240 202, 525, 526, 523, 522, 612, 613, 610, 609 203, 526, 527, 524, 523, 613, 614, 611, 610 204, 527, 183, 182, 524, 614, 262, 263, 611 205, 203, 528, 525, 204, 242, 615, 612, 241 206, 528, 529, 526, 525, 615, 616, 613, 612 207, 529, 530, 527, 526, 616, 617, 614, 613 208, 530, 184, 183, 527, 617, 261, 262, 614 209, 202, 531, 528, 203, 243, 618, 615, 242 210, 531, 532, 529, 528, 618, 619, 616, 615 211, 532, 533, 530, 529, 619, 620, 617, 616 212, 533, 185, 184, 530, 620, 260, 261, 617 213, 201, 534, 531, 202, 244, 621, 618, 243 214, 534, 535, 532, 531, 621, 622, 619, 618 215, 535, 536, 533, 532, 622, 623, 620, 619 216, 536, 186, 185, 533, 623, 259, 260, 620 217, 200, 537, 534, 201, 245, 624, 621, 244 218, 537, 538, 535, 534, 624, 625, 622, 621 219, 538, 539, 536, 535, 625, 626, 623, 622 220, 539, 187, 186, 536, 626, 258, 259, 623 221, 199, 540, 537, 200, 246, 627, 624, 245 222, 540, 541, 538, 537, 627, 628, 625, 624 223, 541, 542, 539, 538, 628, 629, 626, 625 224, 542, 188, 187, 539, 629, 257, 258, 626 225, 198, 543, 540, 199, 247, 630, 627, 246 226, 543, 544, 541, 540, 630, 631, 628, 627 227, 544, 545, 542, 541, 631, 632, 629, 628 228, 545, 189, 188, 542, 632, 256, 257, 629 229, 197, 546, 543, 198, 248, 633, 630, 247 230, 546, 547, 544, 543, 633, 634, 631, 630 231, 547, 548, 545, 544, 634, 635, 632, 631 232, 548, 190, 189, 545, 635, 255, 256, 632 233, 196, 549, 546, 197, 249, 636, 633, 248 234, 549, 550, 547, 546, 636, 637, 634, 633 235, 550, 551, 548, 547, 637, 638, 635, 634 236, 551, 191, 190, 548, 638, 254, 255, 635 237, 195, 552, 549, 196, 250, 639, 636, 249 238, 552, 553, 550, 549, 639, 640, 637, 636 239, 553, 554, 551, 550, 640, 641, 638, 637 240, 554, 192, 191, 551, 641, 253, 254, 638 241, 194, 555, 552, 195, 251, 642, 639, 250 242, 555, 556, 553, 552, 642, 643, 640, 639 243, 556, 557, 554, 553, 643, 644, 641, 640 244, 557, 193, 192, 554, 644, 252, 253, 641 245, 11, 69, 555, 194, 16, 135, 642, 251 246, 69, 70, 556, 555, 135, 134, 643, 642 247, 70, 71, 557, 556, 134, 133, 644, 643 248, 71, 12, 193, 557, 133, 15, 252, 644 249, 285, 645, 103, 14, 286, 648, 37, 9 250, 645, 646, 102, 103, 648, 649, 38, 37 251, 646, 647, 101, 102, 649, 650, 39, 38 252, 647, 281, 13, 101, 650, 290, 10, 39 253, 18, 284, 645, 285, 19, 287, 648, 286 254, 284, 283, 646, 645, 287, 288, 649, 648 255, 283, 282, 647, 646, 288, 289, 650, 649 256, 282, 17, 281, 647, 289, 20, 290, 650 *Nset, nset=_PickedSet8, internal, generate 1, 650, 1 *Elset, elset=_PickedSet8, internal, generate 1, 256, 1 ** Region: (CompositeLayup-1-1: Generated From Layup) *Elset, elset=CompositeLayup-1-1, generate 1, 256, 1 ** Section: CompositeLayup-1-1 *Shell Section, elset=CompositeLayup-1-1, composite, stack direction=3, layup=CompositeLayup-1 0.0003, 3, Stahl, 0., Ply-1 0.00025, 3, CFK, 0., Ply-2 0.0003, 3, Stahl, 0., Ply-1-Copy2 0.00025, 3, CFK, 0., Ply-2-Copy2 0.0003, 3, Stahl, 0., Ply-1-Copy1 0.00025, 3, CFK, 0., Ply-2-Copy1 *End Part ** ** ** ASSEMBLY ** *Assembly, name=Assembly ** *Instance, name=Part-1-1, part=Part-1 0.0, 0., -0.00165 *End Instance ** *Instance, name=Part-1-2, part=Part-1 0.0, 0., 0. *End Instance ** *Nset, nset=_PickedSet10, internal, instance=Part-1-1 11, 12 *Nset, nset=_PickedSet18, internal, instance=Part-1-1 13, 14, 101, 102, 103 *Elset, elset=_PickedSet18, internal, instance=Part-1-1 9, 10, 11, 12, 249, 250, 251, 252 *Nset, nset=_PickedSet19, internal, instance=Part-1-1 1, 2, 21, 22, 23 *Elset, elset=_PickedSet19, internal, instance=Part-1-1 1, 2, 3, 4, 129, 130, 131, 132 *Nset, nset=debond, instance=Part-1-2 1, 2, 13, 14, 15, 16, 17, 18, 21, 22, 23, 101, 102, 103, 104, 105 106, 107, 108, 109, 110, 111, 112, 113, 114, 115, 116, 117, 118, 119, 120, 121 122, 123, 124, 125, 126, 127, 128, 129, 130, 131, 132, 133, 134, 135, 136, 137 138, 139, 140, 141, 142, 143, 144, 145, 146, 147, 148, 149, 150, 151, 152, 153 154, 155, 156, 157, 158, 159, 160, 161, 162, 163, 164, 223, 224, 225, 226, 227 228, 229, 230, 231, 232, 233, 234, 235, 236, 237, 238, 239, 240, 241, 242, 243 244, 245, 246, 247, 248, 249, 250, 251, 252, 253, 254, 255, 256, 257, 258, 259 260, 261, 262, 263, 264, 265, 266, 267, 268, 269, 270, 271, 272, 273, 274, 275 276, 277, 278, 279, 280, 281, 282, 283, 284, 285, 384, 385, 386, 387, 388, 389 390, 391, 392, 393, 394, 395, 396, 397, 398, 399, 400, 401, 402, 403, 404, 405 406, 407, 408, 409, 410, 411, 412, 413, 414, 415, 416, 417, 418, 419, 420, 421 422, 423, 424, 425, 426, 427, 428, 429, 430, 431, 432, 433, 434, 435, 436, 437 438, 439, 440, 441, 442, 443, 444, 445, 446, 447, 448, 449, 450, 451, 452, 453 454, 455, 456, 457, 458, 459, 460, 461, 462, 463, 464, 465, 466, 467, 468, 469 470, 558, 559, 560, 561, 562, 563, 564, 565, 566, 567, 568, 569, 570, 571, 572 573, 574, 575, 576, 577, 578, 579, 580, 581, 582, 583, 584, 585, 586, 587, 588 589, 590, 591, 592, 593, 594, 595, 596, 597, 598, 599, 600, 601, 602, 603, 604 605, 606, 607, 608, 609, 610, 611, 612, 613, 614, 615, 616, 617, 618, 619, 620 621, 622, 623, 624, 625, 626, 627, 628, 629, 630, 631, 632, 633, 634, 635, 636 637, 638, 639, 640, 641, 642, 643, 644, 645, 646, 647 *Elset, elset=debond, instance=Part-1-2, generate 9, 256, 1 *Elset, elset=_Oben_S1, internal, instance=Part-1-2 1, 2, 3, 4, 5, 6, 7, 8, 249, 250, 251, 252, 253, 254, 255, 256 *Elset, elset=_Oben_S2, internal, instance=Part-1-2, generate 9, 248, 1 *Surface, type=ELEMENT, name=Oben _Oben_S1, S1 _Oben_S2, S2 *Elset, elset=_Unten_S1, internal, instance=Part-1-1, generate 9, 248, 1 *Elset, elset=_Unten_S3, internal, instance=Part-1-1, generate 253, 256, 1 *Elset, elset=_Unten_S2, internal, instance=Part-1-1, generate 1, 8, 1 *Surface, type=ELEMENT, name=Unten _Unten_S1, S1 _Unten_S3, S3 _Unten_S2, S2 *End Assembly ** ** MATERIALS ** *Material, name=CFK *Elastic, type=LAMINA 1.23e+11, 8e+09, 0.3, 4.5e+09, 4.5e+09, 4.5e+09 *Material, name=Stahl *Elastic, type=LAMINA 1.75e+11, 1.99e+11, 0.32, 7.2e+10, 7.2e+10, 7.2e+10 ** ** INTERACTION PROPERTIES ** *Surface Interaction, name=IntProp-1 1., *Friction 0., ** ** INTERACTIONS ** ** Interaction: Int-1 *Contact Pair, interaction=IntProp-1, small sliding, adjust=debond Oben, Unten *initial conditions, type=contact Oben, Unten, debond ** ---------------------------------------------------------------- ** ** STEP: Step-1 ** *Step, name=Step-1, nlgeom=YES *Static 1., 1., 1e-05, 1. *debond, slave=Oben, master=Unten, Frequency=1, viscosity=0.1 *FRACTURE CRITERION, TYPE=VCCT, MIXED MODE BEHAVIOR=POWER, tolerance=0.1 228,228,228,1,1,1 ** ** BOUNDARY CONDITIONS ** ** Name: BC-1 Type: Displacement/Rotation *Boundary _PickedSet18, 3, 3 ** Name: BC-2 Type: Displacement/Rotation *Boundary _PickedSet19, 1, 1 _PickedSet19, 3, 3 ** ** LOADS ** ** Name: Load-1 Type: Concentrated force *Cload _PickedSet10, 3, -200. ** ** OUTPUT REQUESTS ** *Restart, write, frequency=0 ** ** FIELD OUTPUT: F-Output-1 ** *Output, field *Node Output CF, RF, U *Element Output, directions=YES LE, PE, PEEQ, PEMAG, S *Contact Output BDSTAT, CDISP, CSTRESS, DBT, EFENRRTR, ENRRT, OPENBC ** ** FIELD OUTPUT: F-Output-2 ** *Output, field *Element Output, elset=Part-1-1.CompositeLayup-1-1, directions=YES, variable=PRESELECT 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16 *Element Output, elset=Part-1-1.CompositeLayup-1-1, directions=YES, variable=PRESELECT 17, 18 *Energy Output, elset=Part-1-1.CompositeLayup-1-1, variable=PRESELECT ** ** FIELD OUTPUT: F-Output-3 ** *Output, field *Element Output, elset=Part-1-2.CompositeLayup-1-1, directions=YES, variable=PRESELECT 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16 *Element Output, elset=Part-1-2.CompositeLayup-1-1, directions=YES, variable=PRESELECT 17, 18 *Energy Output, elset=Part-1-2.CompositeLayup-1-1, variable=PRESELECT ** ** HISTORY OUTPUT: H-Output-1 ** *Output, history, variable=PRESELECT *End Step