enBio-inspired Compliance Grading Motif of Mortar in Nacreous Materials
https://imechanica.org/node/24319
<div class="field field-name-taxonomy-vocabulary-6 field-type-taxonomy-term-reference field-label-hidden"><div class="field-items"><div class="field-item even"><a href="/taxonomy/term/76">research</a></div></div></div><div class="field field-name-taxonomy-vocabulary-8 field-type-taxonomy-term-reference field-label-hidden"><div class="field-items"><div class="field-item even"><a href="/taxonomy/term/12880">nacre</a></div><div class="field-item odd"><a href="/taxonomy/term/3568">additive manufacturing</a></div><div class="field-item even"><a href="/taxonomy/term/12881">spatial material grading</a></div><div class="field-item odd"><a href="/taxonomy/term/8266">bio-inspired materials</a></div><div class="field-item even"><a href="/taxonomy/term/12882">biomimicry</a></div></div></div><div class="field field-name-body field-type-text-with-summary field-label-hidden"><div class="field-items"><div class="field-item even"><p><a href="https://doi.org/10.1021/acsami.0c08181">Bio-inspired Compliance Grading Motif of Mortar in Nacreous Materials</a></p>
<p>J. Ubaid, <a href="https://aeroastro.mit.edu/brian-wardle">B. L. Wardle</a> and <a href="https://www.gla.ac.uk/schools/engineering/staff/kumarshanmugam/">S. Kumar</a></p>
<p>The study demonstrates through experiments (enabled via multi-material additive manufacturing) and computations that compliance grading motifs in the mortar of nacre with optimal spatial gradients, apart from the bulk property mismatch between the brick and mortar and periodic architecture, can allow nacreous materials to be engineered with strong, tough, and damage tolerant properties. For more details, visit the link below.</p>
<p><a href="https://doi.org/10.1021/acsami.0c08181">https://doi.org/10.1021/acsami.0c08181</a></p>
<p>Keywords: nacre, additive manufacturing, spatial material grading, bio-inspired materials, biomimicry</p>