enActuation of Microcantilever Using Light-Driven DNA Conformational Changes
https://imechanica.org/node/11262
<div class="field field-name-taxonomy-vocabulary-6 field-type-taxonomy-term-reference field-label-hidden"><div class="field-items"><div class="field-item even"><a href="/taxonomy/term/76">research</a></div></div></div><div class="field field-name-taxonomy-vocabulary-8 field-type-taxonomy-term-reference field-label-hidden"><div class="field-items"><div class="field-item even"><a href="/taxonomy/term/95">nanomechanics</a></div><div class="field-item odd"><a href="/taxonomy/term/188">Microcantilever</a></div><div class="field-item even"><a href="/taxonomy/term/5717">actuation</a></div><div class="field-item odd"><a href="/taxonomy/term/6737">DNA Motor</a></div><div class="field-item even"><a href="/taxonomy/term/6738">i-motif DNA</a></div><div class="field-item odd"><a href="/taxonomy/term/6739">Conformational Change</a></div><div class="field-item even"><a href="/taxonomy/term/6740">Light Irradiation</a></div></div></div><div class="field field-name-body field-type-text-with-summary field-label-hidden"><div class="field-items"><div class="field-item even"><p>
<strong>Nanomechanical Actuation Driven by Light-Induced DNA Fuel</strong>
</p>
<p>
Kilho Eom, Huihun Jung, Gyudo Lee, Jinsung Park, Kihwan Nam, Sang Woo Lee, Dae Sung Yoon, Jaemoon Yang, and Taeyun Kwon
</p>
<p>
<strong>Abstract</strong>
</p>
<p>
We report the reversible nanomechanical actuation of a microcantilever driven by the light irradiation-induced conformational changes of i-motif DNA chains, which are functionalized on the cantilever's surface. It is shown that light irradiation-driven nanomechanical actuation can be manipulated using DNA hybridization and/or ionic concentrations.
</p>
<p>
</p>
<p>
This work was published online at Chemmical Communications. You can read the paper by clicking the <a href="http://pubs.rsc.org/en/Content/ArticleLanding/2011/CC/C1CC12893K">official website of our paper</a> .
</p>
</div></div></div>Fri, 14 Oct 2011 10:45:13 +0000Kilho Eom11262 at https://imechanica.orghttps://imechanica.org/node/11262#commentshttps://imechanica.org/crss/node/11262Error | iMechanica