I am desperately looking for Postdoc position especially from abroad in the fields of Impact Mechanics, Ballistic load analysis, FRP composite structure, Fracture Mechanics, Numerical modelling and Experimentation etc.

I have completed my Ph.D. with major, "Impact load analysis of FRP composite structure" from Civil Engineering Department, Indian Institute of Technology Roorkee in June 2017. I have published 10 SCI/Scopus Indexed journal papers with total impact factor 17.0.

MM Ansari_IITR's picture

regarding composite modeling under impact

Hi,

i make a model of 3d composite plate with analytical rigid impactor . i used continuum shell element (sc8r element).

my model is not failed even at high velocities. i am not understand why,,,