Please check the consistancy of the units for AA2024T3, which I am using
Thermal Conductivity = 121W/mk
Dencity = 2770 kg/m3
YOungs modulus = 73000000000 N/m2
poisson's ratio = 0.34
Specific heat = 875 J/kg C
Johnson Cook parameters used for Aluminium alloy 2024-T3 (temperature and rate dependent model)
A = 369000000N/m2
B = 684000000N/m2
C = 0.0083
n = 0.73
m= 1.7
Strain rate = 1