Printing, folding and assembly methods for forming 3D mesostructures in advanced materials

Yihui Zhang's picture

Emerging materials and methods for fabricating 3D micro- and nanostructures provide powerful capabilities of relevance across diverse areas of technology. This Review highlights the latest results and future trends associated with the most powerful methods in 3D printing, folding and assembly. 

April Cover of Nature Reviews Materials in 2017

Read the article: Nature Reviews Materials 2, 17019 (2017) (Cover Feature Article)