Freeze casting of novel materials
Fri, 2020-06-19 10:30 - Dr. Hanaor - De...
Freeze casting presents exciting new avenues towards high performance materials with aligned pore structures.
Bone scaffolds, highly elastic composites and nacre mimetic materials can all be produced by means of freeze casting methods.
This comprehensive review presents recent development in terms of materials and processing