Thermo-mechanical model of friction stir welding
My name is Aurelio Tronci and I am a PhD student at the University of Cagliari (Italy). My research topics are related to friction stir welding (FSW). The work done so far has focused on the application of the DOE technique in order to investigate the influence of welding parameters on the microstructural and mechanical properties of aluminum alloys (AA 2198 T3-T8) joints. At the moment I am interested in the development of a thermo-mechanical model of FSW with CFD, but I find it really difficult to find material constants (Sellars and Tegart law) for all the alloys I have to test. Any kind of help in this sense would be very useful!
Thank you.