Evoution of Yield surfaces: Past and Future Trend - Part 2
Submitted by Amit Pandey on Sun, 2010-10-10 21:10.
Continuing on the work from the previous thread posted on
http://imechanica.org/node/9016
Results are presented on the evolution of subsequent yield surfaces with
finite deformation in a very high work hardening annealed 1100 aluminum
alloy. In Part I [Khan, A.S., Kazmi, R., Stoughton, T., Pandey, A.,
2009a. Evolution of subsequent yield surfaces and elastic constants with
finite plastic deformation. Part 1: a very low work hardening aluminum
alloy (Al-6061–T6511) 25, 1611–1625.] of this paper, similar results are
presented for a very low work hardening aluminum alloy.
International Journal of Plasticity, Volume 26, Issue 10, October 2010, Pages 1421-1431
Akhtar S. Khan, Amit Pandey, Thomas Stoughton
»
- Amit Pandey's blog
- Login or register to post comments
- 1772 reads


Recent comments
50 min 11 sec ago
7 hours 41 min ago
17 hours 48 min ago
1 day 18 hours ago
2 days 2 hours ago
2 days 3 hours ago
2 days 13 hours ago
2 days 20 hours ago
3 days 25 min ago
3 days 2 hours ago