VirginiaLFerguson's blog
Journal Club Theme of August 2007: Nanoindentation with focus on soft matter
Submitted by VirginiaLFerguson on Wed, 2007-08-01 07:25.Nanoindentation testing of time-dependent materials is becoming increasingly relevant with advances in areas such as polymer science and the study of materials in biological systems. However, mechanical characterization at micrometer or nanometer length scales is not trivial in such materials that may be highly compliant, heterogeneous, or possess unique morphological characteristics. Although many researchers have made progress in overcoming key challenges that are involved in testing non-traditional materials, significant advancements must still be made to optimize testing methodologies and analytical techniques.
»
- 18 comments
- Read more
- 3727 reads


Recent comments
9 hours 59 min ago
10 hours 36 min ago
13 hours 51 min ago
15 hours 3 min ago
15 hours 25 min ago
15 hours 40 min ago
15 hours 40 min ago
18 hours 39 min ago
22 hours 40 min ago
1 day 46 min ago