adhesive/debond energy

Karl Sieradzki's picture

I am interested in measuring the adhesive energy (debond energy; Turner et al., Acta metall.mater., 43, 3459, 1995) of resin/metal interfaces and am considering several different sample geometries such as the DCDC sample and the double cantilever beam sample. Of course both the resin and metal (e.g., copper) are “ductile” so the situation is different from that for ceramic/metal interfaces. I would like to obtain more reliable numbers for the “adhesive energy” than one might obtain from a simple peel-type test. I am trying to determine if someone has any insights in to the best type of sample configuration for this problem.  Thanks in advance for any suggestions.

Zhigang Suo's picture

Dear Karl:  Have you seen this paper?

S-Y. Kook and R. H. Dauskardt, “Moisture-Assisted Debonding of a Polymer/Metal Interface,” Journal of Applied Physics, 91 [3], 1293-1303, 2002.

Karl Sieradzki's picture

Dear Zhigang: Thanks very much for the reference to the Kook and Dauskardt paper. I had not seen it and it has been very helpful!

Subscribe to Comments for "adhesive/debond energy"

Recent comments

More comments

Syndicate

Subscribe to Syndicate