Computational Study of Cortical Bone Screw Pullout using the Extended Finite Element Method (XFEM) - 2012
Fri, 2012-09-21 16:34 - SIMULIA
In this study, using a UDMGINI subroutine, stress components relative to a predefined osteon orientation were computed and an anisotropic damage criterion was used to determine damage initiation and to predict crack propagation.