Welding simulation

ntuecd's picture

The aim of this tutorial is to develop a step-by-step instructions for simulation of a welding process with the FEA-program LS-PrePost. The tutorial contain a simulation of a single-pass gas metal arc welding, but we can use the same method to simulate multi-pass welding.