Shape memory; ceramics; fracture

mohsenzaeem's picture

A Phase-Field Model for Interactive Evolution of Phase Transformation and Cracking in Super-Elastic Shape Memory Ceramics

This work presents a modified phase-field model for accurate coupling of phase transformation and cracking in shape memory ceramics. The existing phase-field models underestimate the elastic response at the beginning of the mechanical response. We modified the chemical free energy to control the rate of phase transformation and consequently obtain a physical elastic response before initiation of phase transformation. First, the forward and reverse martensitic phase transformation in a superelastic single crystal 3 mol% yttria-stabilized tetragonal zirconia is studied.