Size-dependent analysis

M. Shaat's picture

Effect of Surface Energy on Mechanical Behaviour of Nano Structural Elements

Extremely small size of nano-structures such as beams, sheets and
plates, which are commonly used as components in Nanoelectromechanical Systems
(NEMS), presents a significant challenge to the researchers of nano-mechanics.
Several studies have been developed on the mechanical behavior of nano-sized
bars, tubes, sheets and plates. The results of these studies show that the
elastic modulii of such nano-structural elements depend on their size.
Unfortunately, classical elasticity lacks an intrinsic length scale and thus

Subscribe to RSS - Size-dependent analysis