Influence of depolarization field on polarization states in epitaxial ferroelectric thin films with biaxial misfit strains

Depolarization field and misfit strain are two important factors that may greatly influence the properties of ferroelectric thin films. The effect of depolarization field on polarization states of single-domain ferroelectric thin films with nonequally biaxial in-plane misfit strains are studied in the present work by numerically solving three coupled Euler-Lagrange equations, which are derived from the minimization of total free energy.