On the thermomechanical coupling of shape memory alloys and shape memory alloys composites
Smart materials have received much attention in recent years, especially due to their various applications in smart structures, medical devices, actuators, space and aeronautics. Among these
materials, shape memory alloys exhibit extremely large, inelastic, recoverable strains (of the order of 10%), resulting from transformation between austenitic and martensitic phases. This
transformation may be induced by a change, either in the applied stress, the temperature, or both.