A Comparison of the Elastic Properties of Graphene- and Fullerene-Reinforced Polymer Composites: The Role of Filler Morphology and Size

A recently published paper in mechanical properties of graphene polymer nanocomposites via MD simulations, by Chang-Tsan Lu, Asanka Weerasinghe, Dimitrios Maroudas and Ashwin Ramasubramaniam.