Dynamic necking can avoid notches
Following an earlier post on dynamic necking of tensile bars, we show in the attached paper (to appear in JMPS) that the presence of deep notches in the specimen does not necessarily dictate the location of the neck. Various material parameters are identified and modeled numerically, to assess their respective influence. Strain-rate sensitivity is identified as an important factor.