Measuring Interlayer Shear Stress in Bilayer Graphene Submitted by Zhaohe Dai on Tue, 07/18/2017 - 19:16 research Phys. Rev. Lett. 119, 036101 – Published 17 July 2017 Physics Focus: Graphene Sliding on Graphene Read more about Measuring Interlayer Shear Stress in Bilayer GrapheneLog in or register to post comments3547 views