Skip to main content

almasudme's blog

Need help in Creep modeling in ANSYS

Submitted by almasudme on

Can Anyone help me how to do creep modeling in ansys? 

 

I need to follow the creep law __>      effective creep strain (e at time t) = S. T. e^(-H)

 

S=(a0)^t.(sigma)^(a1) ;     T = t^(a2)+(a3).t^(a4)+(a5)t^(a6)   ; H = (a7)/[(theta)+273.16]

a0 to a7 are material constants.

I have the experimental data and tried to fit the curve in Ansys to obtain the material constants. 