Dynamic compressive behaviour of cellular materials: a review of phenomenon, mechanism and modelling

Submitted by Yongle Sun on

Dynamic compressive behaviour of cellular materials is crucial to their applications in energy absorption, ballistic mitigation and blast/impact protection. The recent research progress in this subject has led to an improved understanding of the experimental, analytical and numerical observations. This review focuses on the aspects ofphenomena, mechanisms and modelling on the concerned subject. Attention is paid to linking macroscopic dynamic compressive behaviour with the subscale influential factors.