Studying the Tensile Behaviour of GLARE Laminates: A Finite Element Modelling Approach

Submitted by Payam Soltani on

By: Payam Soltani, M. Keikhosravy & R. H. Oskouei & C. Soutis 

 http://www.springerlink.com/content/h831735260162p66/

Abstract:

Numerical simulations based on finite element modelling are increasingly being

developed to accurately evaluate the tensile properties of GLARE (GLAss fibre REinforced

aluminium laminates). In this study, nonlinear tensile behaviour of GLARE Fibre Metal