Nonlinear vibration and rippling instability for embedded carbon nanotubes
By: Payam Soltani, D. D. Ganji, I. Mehdipour, A. Farshidianfar
Abstract
By: Payam Soltani, D. D. Ganji, I. Mehdipour, A. Farshidianfar
Abstract
By: M. Keikhosravi, RH Oskouei, Payam Soltani, A. Atas, C. Soutis
Purpose - The main aim of this study is to investigate the effect of geometric variables on the stress and strain distributions as well as non-linear deformation behaviour of aluminium alloy 2024-T3 single-lap bolted joints loaded in tension.
Abstract:
Dear Researchers, Scholars,
We are very glad to inform you about publishing a new quarterly journal, in Multidisciplinary Sciences and Fundamental Physical Sciences as,
“International Journal of Fundamental Physical Sciences (IJFPS)”
Dear Prof/Dr/Colleagues,
With great pleasure and respect to all Prof(s) and Dr(s),
It gives us great pleasure to announce regarding to a new monthly journal publication and online, in Multidisciplinary Sciences, IJFPS.
IJFPS is appreciating, if you submit one of your valuable papers.
IJFPS is your journal and expected to publish in JUN-2011.
IJFPS is hoping for your kind response.
IJFPS is waiting for your submission.
By: Payam Soltani; P. Bahar & A. Farshidianfar
By: Payam Soltani, M. M. Taherian, A. Farshidianfar
http://iopscience.iop.org/0022-3727/43/42/425401
In this study, for the first time, the transverse vibrational model of a viscous-fluid-conveying
single-walled carbon nanotube (SWCNT) embedded in biological soft tissue is developed.
Nonlocal Euler–Bernoulli beam theory has been used to investigate fluid-induced vibration of