Abaqus non linear viscoelasticity and variable strain rates.
Hi ,
I am using abaqus to model a non linear viscoelastic polymer. I have input my relaxation test data as shear data for viscoelastic properties. I have added hyperelastic properties with uniaxial stress strain data as well.
However I find that the results of output stress strain only match for a constant strain rate.