This ebook edition of Mechanics of Fibrous Composites presents the mechanics of fiber-reinforced composite materials. Topics include anisotropy, micromechanics, macromechanical behavior of a lamina, classical lamination theory, failure and dsmage, bending, interlaminar stresses,laminated tubes, test methods, material response, and related aspects of the mechanical behavior of fibrous composites. The book emphasizes the development and application of the fundamental equations governing laminated composite materials and structures. This ebook edition is made freely available by the author.