Analysis of the Rate-Dependent Coupled Thermo-Mechanical Response of Shape Memory Alloy Bars and Wires in Tension

Submitted by arash_yavari on

In this paper, the coupled thermo-mechanical response of shape memory alloy (SMA) bars and wires in tension is studied.It is shown that the accuracy of assuming adiabatic or isothermal conditions in the tensile response of SMA bars strongly depends on the size and the ambient condition in addition to the rate-dependency that has been known in the literature.