Hi everyone
Does anyone know about tension stiffening of concrete. Actually I have a problem with getting these values. i have an example of it and I wanna show you to clarify. So, the given information is as follows:
E= 31027 mpa
V= 0.15
Density= 2663 kg/m3
Compressive initial stress= 13 mpa
Compressive ultimate stress= 24.1 mpa
Tensile failure stress= 2.9 mpa
Therefore, for mentioned above "tensile behavior" in terms of dis. is as following: ( concrete damage plasticity )
Yield stress. Displacement
2900000 0
1943930 6.6185E-005
1303050 0.00012286
873463 0.000173427
585500 0.00022019
392472 0.000264718
263082 0.000308088
176349 0.00035105
118210 0.000394138
79238.8 0.000437744
53115.4 0.000482165
Hence, for tension stiffening ( concrete tension damage ) following values are taken:
Damage parameters. Displacement
0. 0
0.381217. 6.61E-005
0.617107. 0.00012286
0.76307. 0.000173427
0.853393. 0.00022019
0.909282. 0.000264718
0.943865. 0.000308088
0.965265. 0.00035105
0.978506. 0.000394138
0.9867. 0.000437744
0.99177. 0.000482165
___________________________________________________
So my properties are as following:
E= 23000 mpa
V= 0.2
Density= 2386 kg/m3
Compressive initial stress= 13 mpa
Compressive ultimate stress= 20 mpa
Tensile failure stress= 2.5 mpa
Please help me to find the values.
KHALED GHAEDI
Sincerely yours; PASOFAL
Sincerely yours;
PASOFAL