How can a zero length torsional spring element be modeled in ANSYS?

Aoa

Hello
brothers

Currently,
I‘m working on the determination of the mechanical properties of carbon nanotubes
for different loading cases using ANSYS software ( i need to use them in my
model). My Finite Element model of graphene and carbon nanotube is working fine with beam188 element, but I have
some technical problems in my simulation. These problem are summarized in
points as follow;

  •  I want to replace the beam element by two springs (linear torsional spring and nonlinear
    stretching spring element). Each spring will produce one type
    of deformation in the nanotube. The problem is with the torsional spring that
    must be modeled as a zero length element. So, which element can be used in this
    case and it can provide a properties for zero length element?
  • If there is an element that can be used as it described above, can anyone one help
    me to understand the theory  of the element?

Thank you

Moosa  S.M. Al Kharusi

Subscribe to Comments for "How can a zero length torsional spring element be modeled in ANSYS?"

Recent comments

More comments

Syndicate

Subscribe to Syndicate
Error | iMechanica

Error

The website encountered an unexpected error. Please try again later.