Dynamic Rolling Process FE Simulation

Submitted by Hassan Nazari on

 

Dear All,

 

I hope all feel so fine with your simulations.

 

Recently, I am simulation a rolling process with a very high dynamic speed (around 5 m/s). Hence, the model is quite dynamic and not Quasi-static.

 

I use Abaqus Explicit for this simulation. The structure is composite material including several layers with different material properties. In this case, I am using ''Cohesive Surface'' definition as the surface interaction between different layers.

 

 

 

I have a big problem and there is an error during the simulation process so called:

 

 ''the ratio of deformation speed to wave speed exceeds 1.0000 in at least one element''.

 

I tried to find a solution for this problem such as:

 

Larger mesh โ€ฆโ€ฆ. But the larger mesh decreases the solution accuracy.

 

Have you ever seen any solution for this case?

 

In this respect, may I imagine to let me know please if you have already any hints or solution for this problem.

 

 

 

Thanks for your attention.

 

Kind regards,

 

Hassan