Skip to main content

ABD matrix and Effective Properties of Composite Laminates

Submitted by Hamsasew on

Mechanics of structure genome (MSG) is a powerful tool that helps to obtain both effective properties and ABD matrix of composite laminates. The example shown here is how to predict the effective properties and ABD matrix of composite laminates starting from microstructural details of the composite.    

 