Our new work presents tests of an unprecedented range of specimen sizes for studying size effect in cementitious materials. Foe evreyone interested, a paper about it has been published in Cement and Concrete Composites. It is available at:https://www.researchgate.net/publication/327876010_Size_effect_on_splitโฆ;