You are here
Reinforced Concrete Slab Optimization with Simulated Annealing
Mon, 2019-08-05 02:33 - Flavio Stochino
I am glad to to share a new paper published on Applied Sciences. An optimization method, based on Simulated Annealing, is developed for the design of reinforced concrete slab.
Find out more at: https://www.mdpi.com/2076-3417/9/15/3161
https://www.academia.edu/40011194/Reinforced_Concrete_Slab_Optimization_with_Simulated_Annealing hashtag
#engineering hashtag#research hashtag#structuralengineering hashtag#concrete hashtag#reinforcedconcrete hashtag#structuraldesign