New results on shock mitigation of MC gels to appear in JMPS

Submitted by D.Rittel on

This recently accepted paper, to appear in the Journal of the Mechanics and Physics of Solids, reports our detailed experiments on shock energy absorption of methylcellulose hydrogels. A phenomenological model is developed and validated that allows for a quantitative estimate of the attnuated signal as a function of the gel layer thickness and composition.