A new performance measure in piezoelectricity! This paper presents the notion of "energy-harvesting availability" -- an intrinsic material-level measure for piezoelectric energy-harvesting characterization. This contrasts with the prevailing approach of extrinsic characterization done at the structural or device levels.
Article is freely available at:
Smart Mater. Struct. 30, 085022, 2021
https://iopscience.iop.org/article/10.1088/1361-665X/ac0c2c