Semiflexible polymer chain under sustained tension as a model of cytoskeletal rheology
Wed, 2006-11-29 15:57 - Dimitrije Stamenovic
This is a model of a single semiflexible polymer chain under sustained tension. The model captures two key features of the cytoskeletal rheology: a) the power-law behavior; and b) the dependence of the power-law on mechanical prestress. The model also reveals the underlying mechanisms.