In the attached paper, we propose a procedure combining an XFEM/level-set technique and Gurtin-Murdoch surface elasticity to model nanostructures with arbitrary geometries. The effects of free surface which are dominant at small scales are easily captured in this framework.
| Attachment | Size |
|---|---|
| [18] nanoXFEM.pdf | 1.4 MB |