A question how is possible in the same material and in the same temprature we observe some different material properties? as we can see in shape alloy effect? I appreciate if somebody give me some clues as a light to shed the research way. thank you in advance.
Hi phase transformation
Hi
phase transformation of microstructures (from austinite to martensite and vise cersa) takes place which leads to generation of strain or force if restrained. the phase transformation of ice to liquid water happens in the same matrial and same temprature.