Skip to main content

Composite laminate

Submitted by vinay kumar B A on

 

hi all..

 

i am interested to solve composite laminate problem, but i am not getting
the proper results, i request you to send any ansys tutorial if you
have.





thanking you





vinay.

 

vinay.kumar233 [at] gmail.com

 

vinay_kumar233 [at] yahoo.com

 

 

Hi,

what do you mean with "I do not get the proper results"? One very important thing in composites is to ensure that you have build properly the composite material, that means, that the different elements of your model are oriented properly. That is normally introduced iin the input file using a different ommand. That is very diffiult to get directly in all preprocessors I know unless special tools are used, like Laminate Modeller in PATRAN or Composite in Hypermesh. 

Best regards,

Mikel

Sat, 04/10/2010 - 13:25 Permalink