I need to model viscoelastic behavior of polymer. I have storage modulus and loss modulus data as a function of temperature. I have found to determine the Prony series coefficients Ansys need shear and bulk modulus as a function of time-temperature. Does it mean complex shear moduls which can be calculated from storage and loss modulus. Can anyone advise me how I can use my data to calculate Prony series coefficients using Ansys?
Hi, Â I am working on a
Hi,
I am working on a similar topic and was wondering if you got the solution to how to evaluate the prony series coefficients? I have a stress- strain curve of the material. Would that be sufficient?.
Thanks
requesti
Hello , i am working on similar project if hv already finished ur project let me know details,,,,,,,,,,,,,,,,pls help in doing this project,,,,,,,,,,,,,,,