Submitted by tzirakian on Wed, 08/11/2010 - 07:11 I would like to know the amount of increase of steel shear modulus under pressure or compression. Any ideas, references, ... I'd appreciate your support in advance. Thanks. Biswajit Banerjee Re: Steel shear modulus as a fn of pressure Take a look at: The Mechanical Threshold Stress Model for various tempers of AISI 4340 steel , International Journal of Solids and Structures., vol 44, no. 3-4, pp. 834-859. -- Biswajit Log in or register to post comments Wed, 08/11/2010 - 22:17 Permalink tzirakian Increase of steel shear modulus under pressure/compression Thanks a lot for your support. Log in or register to post comments Thu, 08/12/2010 - 20:02 Permalink Log in or register to post comments4698 views
Biswajit Banerjee Re: Steel shear modulus as a fn of pressure Take a look at: The Mechanical Threshold Stress Model for various tempers of AISI 4340 steel , International Journal of Solids and Structures., vol 44, no. 3-4, pp. 834-859. -- Biswajit Log in or register to post comments Wed, 08/11/2010 - 22:17 Permalink
tzirakian Increase of steel shear modulus under pressure/compression Thanks a lot for your support. Log in or register to post comments Thu, 08/12/2010 - 20:02 Permalink
Re: Steel shear modulus as a fn of pressure
Take a look at:
The
Mechanical Threshold Stress Model for various tempers of AISI 4340
steel , International Journal of Solids and Structures., vol 44, no.
3-4, pp. 834-859.
-- Biswajit
Increase of steel shear modulus under pressure/compression
Thanks a lot for your support.