Rapid Solidification; Phase-field modeling

Quantitative Phase-Field Modeling of Solute Trapping in Rapid Solidification

Submitted by mohsenzaeem on

A quantitative phase-field model is developed for prediction of solute trapping for solidification velocities relevant to additive manufacturing. S. Kavousi and M. Asle Zaeem, Quantitative phase-field modeling of solute trapping in rapid solidification.  Acta Materialia 205 (2021) 116562 (11 pages).