Entropic rigidity of a crumpling network in a randomly folded thin sheet

Submitted by Balankin on

We have studied experimentally and theoretically the response of randomly folded hyperelastic and elastoplastic sheets on the uniaxial compression loading and the statistical properties of crumpling networks. The results of these studies reveal that the mechanical behavior of randomly folded sheets in the one-dimensional stress state is governed by the shape dependence of the crumpling network entropy.