Determination of Representative Volume Element (RVE) based on Microstructure
Estimating the response of polycrystalline materials using sets of weighted statistical volume elements
Siddiq M. Qidwai, David M. Turner, Stephen R. Niezgoda, Alexis C. Lewis, Andrew B. Geltmacher, David J. Rowenhorst, Surya R. Kalidindi
Acta Materialia, 60, 5284โ5299, 2012; http://dx.doi.org/10.1016/j.actamat.2012.06.026