Pseudomagnetic Fields in a Locally Strained Graphene Drumhead

Submitted by Shuze Zhu on

Recent experiments reveal that a scanning tunneling microscopy (STM) probe tip can generate a highly localized strain field in a graphene drumhead, which in turn leads to pseudomagnetic fields in the graphene that can spatially confine graphene charge carriers in a way similar to a lithographically defined quantum dot (QD). While these experimental findings are intriguing, their further implementation in nanoelectronic devices hinges upon the knowledge of key underpinning parameters, which still remain elusive.