How human bone repairs itself Submitted by Mogadalai Gururajan on Tue, 04/17/2007 - 06:53 biomechanics damage mechanics In a recent Progress Article in Nature Materials, David Taylor, Jan G Hazenberg, and T Clive Lee write about the damage that human bones sustain as a result of cyclic stresses under which they operate and the repair mechanisms that operate. Read more about How human bone repairs itselfLog in to post comments7251 views