Strengthening alginate/polyacrylamide hydrogels using various multivalent cations

Submitted by _canhuiyang on
We successfully synthesized a family of alginate/polyacrylamide hydrogels using various multivalent cations. These hydrogels exhibit exceptional mechanical properties. In particular, we found that the hydrogels cross-linked by trivalent cations are much stronger than those cross-linked by divalent cations. We demonstrate stretchability and toughness of the hydrogels by in๏ฌ‚ating a hydrogel sheet